Improving degradation of polyethylene /acrylic dextrose with ground nut powder
Improving degradation of polyethylene /acrylic dextrose with ground nut powder

Santhoskumar A. Umapathi; Jaya Chitra Natarajan

Volume 4, Issue 1 , January and February 2020, , Pages 100-105

https://doi.org/10.33945/SAMI/CHEMM.2020.1.9

Abstract
  The novel bio-based additives in the present research were incorporated into LDPE, LDPE in about 5 wt% subsequently processed to produce films of 50μ thickness. The bio-based additive ...  Read More
Studies on Isora Fibers Mixed with 1% Ricinoleic Acid Reinforced with Polypropylene
Studies on Isora Fibers Mixed with 1% Ricinoleic Acid Reinforced with Polypropylene

A.U Santhoskumar; N. Jaya Chitra

Volume 3, Issue 6 , November and December 2019, , Pages 713-720

https://doi.org/10.33945/SAMI/CHEMM.2019.6.9

Abstract
  The aim of this study is to investigate the effectiveness of Isora fiber mixed with 1% ricinoleic acid as a reinforcement for polypropylene (PP) thermoplastic matrix. Isora fibers were ...  Read More
Studies on Mechanical and Thermal Properties of PP with Natural Carbon Powder
Studies on Mechanical and Thermal Properties of PP with Natural Carbon Powder

A.U Santhoskumar; N. Jaya Chitra

Volume 3, Issue 3 , May and June 2019, , Pages 340-347

https://doi.org/10.22034/chemm.2018.147034.1082

Abstract
  The work has to develop polypropylene (PP) mixed for the purpose of compatible into the Prosopis juliflora bark powder (PB), Wheat husk carbon powder (WC) and Banyan carbon powder (BBC) ...  Read More
Structural Characteristics Changes after the Degradation of Polyethylene with Cobalt 12-Hydroxy Oleate Acrylic Dextrose
Structural Characteristics Changes after the Degradation of Polyethylene with Cobalt 12-Hydroxy Oleate Acrylic Dextrose

A. Umapathi Santhoskumar; N. Jaya Chitra

Volume 3, Issue 1 , January 2019, , Pages 83-93

https://doi.org/10.22034/chemm.2018.135055.1062

Abstract
  The novel bio-based additives synthesized in the present research were incorporated into LDPE, LDPE in about 1-5 wt % subsequently processed to produce films of 50 μ thickness. The ...  Read More